 Verfasst am: Sa Jan 22, 2011 5:44 am Titel: Make your own plastic groundglass |
|
 Verfasst am: Sa Jan 22, 2011 5:44 am Titel: Make your own plastic groundglass |
|
|
luisalegria wrote:
Anybody who has played around with OLD cameras has probably run into the situation where a new prize plate camera, press camera or folder turns out to be missing its groundglass, or the old one is cracked. Replacement groundglass can cost $15-50 depending on where you look.
Its also common to need to adjust infinity on old folders, etc., for which a groundglass across the film mask is essential.
There are plenty of workarounds for that job, such as clear tape, but its best to have a rigid piece with better visual quality.
Making a glass groundglass yourself is very possible, but its a pain in the bottom and takes longer than one would think. And I don't like the ones I've made. And I can't get the things to ever break neatly.
A few weeks ago I bought a large (2'x4') piece of 1/16" (1.5mm) acrylic from TAP Plastics - http://tapplastics.com/
These sheets come with masking plastic film on both sides.
And a few pieces of Tamiya 800-grit sandpaper. This is used for sanding styrene plastic on model kits.
Cut out a piece of plastic of the right size -the proper size to replace a glass groundglass, or to fit over a cameras film gate - I have made pieces to fit on most 6x9, 6x7, 6x6, 4.5x6 and 35mm.
Cutting is very easy. I use a cutting wheel on my dremel, but a hacksaw with a fairly fine-toothed blade is just fine. Sand the edges until they are smooth, so the piece will lie flat.
Peel off the masking film from one side.
Sand that side with the sandpaper. Best to use a sanding block. It doesn't matter very much what pattern you use. Just sand it until its translucent. It will not take long at all.
Wash the piece.
Peel the film from the other side.
And there you are, a groundglass, better than any glass one, most likely, that you will make in your first few tries. And you can make any size or shape. _________________ I like Pentax DSLR's, Exaktas, M42 bodies of all kinds, strange and cheap Japanese lenses, and am dabbling in medium format/Speed Graphic work. |
|
| Nach oben |
|
 |
TBaker
 Anmeldungsdatum: 02.12.2009 Beiträge: 344 Wohnort: Canada
|
 Verfasst am: Sa Jan 22, 2011 12:05 pm Titel: |
|
 Verfasst am: Sa Jan 22, 2011 12:05 pm Titel: |
|
|
TBaker wrote:
Couldn't you use liquid etch on real glass to get the matt look? |
|
| Nach oben |
|
 |
Sevo
 Anmeldungsdatum: 22.08.2008 Beiträge: 1189 Wohnort: Frankfurt, Germany
Expire: 2012-12-03
|
 Verfasst am: Sa Jan 22, 2011 12:39 pm Titel: |
|
 Verfasst am: Sa Jan 22, 2011 12:39 pm Titel: |
|
|
Sevo wrote:
| TBaker hat folgendes geschrieben:: |
| Couldn't you use liquid etch on real glass to get the matt look? |
You could. However the "etch" are hydrogen fluoride fumes, one of the most effective means to reduce your lung capacity finally and fatally. With abrasives you get much better control (the grain corresponds to the sandpaper grain rather than the flow of HF fumes) at no risk at all. _________________ Sevo |
|
| Nach oben |
|
 |
poilu
 Anmeldungsdatum: 26.08.2007 Beiträge: 10476 Wohnort: Greece
Expire: 2019-08-29
|
 Verfasst am: Sa Jan 22, 2011 2:27 pm Titel: |
|
 Verfasst am: Sa Jan 22, 2011 2:27 pm Titel: |
|
|
poilu wrote:
great trick, I will try it _________________ T* |
|
| Nach oben |
|
 |
cooltouch
 Anmeldungsdatum: 15.01.2009 Beiträge: 9096 Wohnort: Houston, Texas
|
 Verfasst am: Sa Jan 22, 2011 5:34 pm Titel: |
|
 Verfasst am: Sa Jan 22, 2011 5:34 pm Titel: |
|
|
cooltouch wrote:
I have a portable sand blaster rig that I've thought about doing this with before, but now that I think about it, the sand particle size is probably too large. 800 grit or finer sounds like a better solution. I have some clear plastic scrap laying about that I think I'll give it a try with. I also have some rather special sand paper, called Micro Mesh, that was originally designed for use to polish out acrylic aircraft windows that might become abraded after years of flying. It comes in grits from 1500 to 12000. The 1500 grit may be scratchy enough to give the ground glass translucence.
I was thinking about this recently as a way of checking the accuracy of a SLR camera/lens combination's focus compared to what one sees in the viewfinder. But it's nice to know about should I ever run across an old view camera for cheap because its ground glass is busted. _________________ Michael
My Gear List: http://michaelmcbroom.com/photo/gear.html
My Gallery: http://michaelmcbroom.com/gallery3/index.php/
My Flickr Page: https://www.flickr.com/photos/11308754@N08/albums
My Music: https://soundcloud.com/michaelmcbroom/albums
My Blog: http://michaelmcbroom.com/blogistan/ |
|
| Nach oben |
|
 |
marty
 Anmeldungsdatum: 09.04.2009 Beiträge: 767 Wohnort: Italy
|
 Verfasst am: Sa Jan 22, 2011 6:26 pm Titel: |
|
 Verfasst am: Sa Jan 22, 2011 6:26 pm Titel: |
|
|
marty wrote:
Thank for sharing, Luis. Sounds like a great idea.
Cheers, M. _________________ Canon FD
Bodies: AT-1, A-1, T-90
Lenses: nFD 20mm f2.8, 24 f2.8, 28 f2.8, 35 f2, FD 50 f1.8 S.C., 85 f1.8, 100 f2.8, 135 f2.8, 200 f4, 300 f4
|
|
| Nach oben |
|
 |
|
|
|
Du kannst keine Beiträge in dieses Forum schreiben. Du kannst auf Beiträge in diesem Forum nicht antworten. Du kannst deine Beiträge in diesem Forum nicht bearbeiten. Du kannst deine Beiträge in diesem Forum nicht löschen. Du kannst an Umfragen in diesem Forum nicht mitmachen.
|